Case Study: Aluminum Foil Slitter
A Vietnamese converter slitting 30 µm aluminium foil at 400 m/min was getting 5 days from a D2 slitter. The fix was a M2 HSS slitter with a ta-C coating.

A Vietnamese converter slitting 30 µm aluminium foil at 400 m/min was getting 5 days from a D2 slitter. The fix was a M2 HSS slitter with a ta-C coating.

A Polish converter cutting 12 µm BOPP film at 600 m/min was burning through 4 D2 slitters per week. The fix was a 2-week field audit, a steel-grade change.